Chemical Composition
0.25 to 0.5
%    
23 to 26
%    
55.2 to 64.8
%    (estimate)
2.5
%  (maximum)  
12 to 14
%    
0.04
%  (maximum)  
0.04
%  (maximum)  
1.75
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
235
10^7 dyne/cm^2  (minimum)  
490
10^7 dyne/cm^2  (minimum)  
8
% strain  (minimum)  
 
Other Information