Chemical Composition
0.15
%  (maximum)  
11.5 to 14
%    
0.5
%  (maximum)  
81.2 to 88.5
%    (estimate)
1
%  (maximum)  
0.5
%  (maximum)  
1
%  (maximum)  
0.04
%  (maximum)  
0.04
%  (maximum)  
1.5
%  (maximum)  
0.1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
448
10^7 dyne/cm^2  (minimum)  
620 to 792
10^7 dyne/cm^2    
18
% strain  (minimum)  
 