Chemical Composition
0.1
%  (maximum)  
16.5 to 17.5
%    
74.9 to 77
%    (estimate)
2.5 to 3
%    
4 to 4.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
310 to 979
10^7 dyne/cm^2    
1110 to 1380
10^7 dyne/cm^2    
8 to 22
% strain    
200 to 390
   
 
Other Information
Links