Chemical Composition
0.9 to 1.35
%    
0.05
%  (maximum)  
12.3 to 13.3
%    
0.2
%  (maximum)  
2 to 2.5
%    
7.5 to 8.5
%    
0.01
%  (maximum)  
0.008
%  (maximum)  
0.1
%  (maximum)  
 
Mechanical Properties
DimensionsYield Strength (Pa)Ultimate Tensile Strength (Pa)Elongation (% strain)Brinell Hardness
Thickness, 12 in. max≥ 1.41e9≥ 1.52e9≥ 10≥ 430

1.41e9
Pa  (minimum)  
1.52e9
Pa  (minimum)  
10
% strain  (minimum)  
430
 (minimum)  
 
Other Information
Links
 



No warranty is given for the accuracy of these data