Layout: Alloy Finder
View
Full datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
SI (Consistent)
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
Metric
UK Imperial
US Customary
Structural high-strength steel, AERMET 100 ALLOY (Carpenter Technology Corp.)
add data link
Chemical Composition
Base Element
Fe (Iron)
C (Carbon)
0.23
%
Co (Cobalt)
13.4
%
Cr (Chromium)
3.1
%
Fe (Iron)
71
%
(estimate)
Mo (Molybdenum)
1.2
%
Ni (Nickel)
11.1
%
Balance
Fe (Iron)
Composition Note
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Mechanical Properties
Yield Strength
1.69e9 to 1.76e9
Pa
Ultimate Tensile Strength
1.93e9 to 2e9
Pa
Elongation
14 to 16
% strain
Other Information
Material Class
Ferrous Alloy
Alloy Family
High-Strength Steel
Alloy Group
Structural
Country
USA
Designation
AERMET 100 ALLOY
Specification Type
Manufacturer's Specification
Similar UNS Number
K92580
Source
Manufacturer's Datasheet
Online Source
Online Datasheet
Organization
Carpenter Technology Corp.
Similar Alloys
Click here to find similar alloys
Links
Organizations
Carpenter Technology Corp.
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard