Chemical Composition
0.02
%  (maximum)  
19.5 to 20.5
%    
0.5 to 1
%    
1
%  (maximum)  
6 to 6.5
%    
17.5 to 18.5
%    
0.03
%  (maximum)  
0.01
%  (maximum)  
0.8
%  (maximum)  
N2C = 0.18 to 0.22
 
Mechanical Properties
DimensionsYield Strength (Pa)Ultimate Tensile Strength (Pa)Elongation (% strain)
None Specified≥ 3.03e86.48e8 to 8.2e8≥ 28

3.03e8
Pa  (minimum)  
6.48e8 to 8.2e8
Pa    
28
% strain  (minimum)  
Elongation in 4 D
 
Other Information
Links
 



No warranty is given for the accuracy of these data