Chemical Composition
0.2 to 0.6
%    
28 to 32
%    
40.8 to 53.8
%    (estimate)
2
%  (maximum)  
0.5
%  (maximum)  
18 to 22
%    
0.04
%  (maximum)  
0.04
%  (maximum)  
2
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
2.4e8
Pa  (minimum)  
4.5e8
Pa  (minimum)  
10
% strain  (minimum)  
 