Range attributes
360 to 385
   
0.35
%    
0.42
%    
16
% strain    
96.7
%    (estimate)
1.92
%    
0.32
%    
0.28
%    
1.08e9
Pa    
1.01e9
Pa    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Heat treated: 157,000 TS; 146,000 YS; 16 El; 58 RA; 360-385 HB; For chutes, hoppers, conveyors, screens, liners, scrapers, buckets; wear and impact resistant, mill heat treated.
MANGABRAZE
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Heat treated: 157,000 TS; 146,000 YS; 16 El; 58 RA; 360-385 HB; For chutes, hoppers, conveyors, screens, liners, scrapers, buckets; wear and impact resistant, mill heat treated.
 