Wrought bronze, CUPRONAR 950 (Arcos Alloys Corp.)
add data link
Range attributes
Al (Aluminum)
6 to 9
%
Cu (Copper)
90.9 to 93.9
%
(estimate)
Si (Silicon)
0.1
%
Logical attributes
Wire
Yes
Discrete attributes
~Checking Status
Not verified - Original build
Date Last Checked
Thursday, October 17, 2013
Available forms
Wire
Balance
Cu (Copper)
Base Element
Cu (Copper)
Country
USA
Material Class
Nonferrous Alloy
Source
Woldman's Engineering Alloys 9th ed. J. Frick Editor, ASM International 2000
Specification Status
Obsolete
Specification Type
Manufacturer's Specification
Short text attributes
Composition Note_old
Cu is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Country*
USA
Description_old
For welding wires; aluminum bronze, AWS ECuAl-Al.
Designation
CUPRONAR 950
Long text attributes
Composition Note
Cu is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Description
For welding wires; aluminum bronze, AWS ECuAl-Al.
Hyperlink attributes
Similar Alloys
Click here to find similar alloys
Integer attributes
ID
67131
Source ID
232074
Further Information
Organizations
Arcos Alloys Corp.
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard