Steel castings, stainless, precipitation hardening; PH Heat Treatment H1150
ASME International (ASME)
 
Hyperlink attributes
Integer attributes
Tabular attributes
DimensionsYield Strength (Pa)Ultimate Tensile Strength (Pa)Elongation (% strain)Brinell HardnessRockwell 30-T scaleTreatmentHardness ScaleVickers hardness (HV)
None Specified≥ 6.69e8≥ 8.62e8≥ 10≥ 269    

 