Range attributes
0.25
%  (maximum)  
24 to 30
% strain    
98.5 to 98.8
%    (estimate)
1
%    
0.25
%    
4.48e8 to 5.52e8
Pa    
2.41e8 to 3.45e8
Pa    
 
Logical attributes
Yes
Yes
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Cast: 65,000-80,000 TS; 35,000-50,000 YP; 24-30 El; 35-50 RA. For general and structural applications, gears, shafts, housings. AISI 4024 modified. Tough.
BIRDSBORO-CMO
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Cast: 65,000-80,000 TS; 35,000-50,000 YP; 24-30 El; 35-50 RA. For general and structural applications, gears, shafts, housings. AISI 4024 modified. Tough.
 