Chemical Composition
0.08 to 0.15
%    
4.5 to 5.5
%    
92.6 to 94.4
%    (estimate)
0.3 to 0.6
%    
0.45 to 0.55
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.3 to 0.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
2.45e8
Pa    
4.4e8 to 5.9e8
Pa    
20
% strain    
130 to 175
   
 
Other Information