Chemical Composition
0.2
%  (maximum)  
97.6 to 100
%    (estimate)
1.6
%  (maximum)  
0.009
%  (maximum)  
0.04
%  (maximum)  
0.04
%  (maximum)  
0.55
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
2.95e8
Pa    
4.7e8 to 6.3e8
Pa    
18
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data