Chemical Composition
0.34
%    
0.82
%    
96.9
%    (estimate)
0.78
%    
0.4
%    
0.28
%    
0.51
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1.28e9 to 1.49e9
Pa    
1.34e9 to 1.84e9
Pa    
37 to 51
% strain    
395 to 498
   
 
Other Information
Heat treated: 194,000-267,000 TS; 185,000-216,000 YS; 37-51 El; 9-15 RA; 395-498 HB; For arbors, dies, gears, shafts, spindles; oil or water hardened, non-tempering.