Chemical Composition
0.15 to 0.3
%    
0.03
%    
71.5 to 73.5
%    (estimate)
0.5
%  (maximum)  
25 to 26
%    
1.3 to 1.6
%    
0.02
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1.46e9 to 1.7e9
Pa    
1.65e9 to 1.83e9
Pa    
3 to 5
% strain    
 
Other Information
Heat treated: 240,000-265,000 TS; 212,000-246,000 YS; 3-5 El. For rocket motor cases, airframes, airborne equipment, large machinery parts, bolts, cryogenic equipment, high temperature equipment. Maraging steel, shock resistant.