Layout: Alloy Finder
View
Summary datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
SI (Consistent)
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
Metric
UK Imperial
US Customary
(2xxx series) wrought aluminum-copper, BIRMETAL BMB 478 (Birmetals Ltd.)
add data link
Chemical Composition
Base Element
Al (Aluminum)
Al (Aluminum)
93.4
%
(estimate)
Cu (Copper)
4.3
%
Mg (Magnesium)
0.7
%
Mn (Manganese)
0.8
%
Si (Silicon)
0.8
%
Balance
Al (Aluminum)
Composition Note
Al is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Mechanical Properties
Yield Strength
3.1e8
Pa
Ultimate Tensile Strength
4.4e8
Pa
Elongation
18
% strain
Vickers Hardness
1.18e9
Pa
Other Information
Material Class
Nonferrous Alloy
Country
United Kingdom
Description
Sheet and strip: 440 MPa TS; 310 MPa YS; 18 El; 120 HV (TB condition). AA 2014.
Designation
BIRMETAL BMB 478
Specification Type
Manufacturer's Specification
Specification Status
Obsolete
Source
Woldman's Engineering Alloys 9th ed. J. Frick Editor, ASM International 2000
Available forms
Sheet
,
Strip
Similar Alloys
Click here to find similar alloys
Links
Organizations
Birmetals Ltd. (Birmabright Works)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard