Layout: Alloy Finder
View
Full datasheet
Printable datasheet
Hide empty items
Record properties
Expand headings
Collapse headings
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
US Customary
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
Metric
SI (Consistent)
UK Imperial
CB7Cu-2 Type 15-5, ASME SA747/SA747M, Casting; H1150
add data link
Chemical Composition
Base Element
Fe (Iron)
Ag (Silver)
Al (Aluminum)
As (Arsenic)
Au (Gold)
B (Boron)
Be (Beryllium)
Bi (Bismuth)
C (Carbon)
0.07
% (maximum)
Ca (Calcium)
Cd (Cadmium)
Ce (Cerium)
Co (Cobalt)
Cr (Chromium)
14 to 15.5
%
Cu (Copper)
2.5 to 3.2
%
Fe (Iron)
Ga (Gallium)
Hf (Hafnium)
In (Indium)
Li (Lithium)
Mg (Magnesium)
Mn (Manganese)
0.7
% (maximum)
Mo (Molybdenum)
N (Nitrogen)
0.05
% (maximum)
Na (Sodium)
Nb (Niobium)
0.15 to 0.35
%
Ni (Nickel)
4.5 to 5.5
%
P (Phosphorus)
0.035
% (maximum)
Pb (Lead)
Pd (Palladium)
Pt (Platinum)
S (Sulfur)
0.03
% (maximum)
Sb (Antimony)
Se (Selenium)
Si (Silicon)
1
% (maximum)
Sn (Tin)
Sr (Strontium)
Ta (Tantalum)
Te (Tellurium)
Th (Thorium)
Ti (Titanium)
Tl (Thallium)
V (Vanadium)
W (Tungsten)
Zn (Zinc)
Zr (Zirconium)
Balance
Others Total
Others Each
Other elements
Composition Note
Mechanical Properties
Tabular Data
Hide table
Save as CSV
Copy To Clipboard
Dimensions
Yield Strength (ksi)
Ultimate Tensile Strength (ksi)
Elongation (% strain)
Brinell Hardness
Rockwell 30-T scale
None Specified
≥ 97
≥ 125
≥ 10
≥ 269
Save as CSV
Copy To Clipboard
Yield Strength
97
ksi (minimum)
Ultimate Tensile Strength
125
ksi (minimum)
Elongation
10
% strain (minimum)
Density
Brinell Hardness
269
(minimum)
Vickers Hardness
Rockwell Hardness C scale
Rockwell Hardness B scale
Rockwell Hardness A scale
Rockwell 30-T scale
Rockwell 15-T scale
Condition
Notes on Mechanical Properties
Other Information
Material Class
Ferrous Alloy
Alloy Family
High-Alloy Steel (Corrosion and Heat Resistant, Stainless, and Nickel Steels)
Alloy Group
Precipitation-hardening stainless steel
Alloy Sub-Group
Miscellaneous precipitation-hardening steels
Country
USA
Standards Body
ASME (USA)
Description
Steel castings, stainless, precipitation hardening; PH Heat Treatment H1150
Alternate Name
Designation
CB7Cu-2 Type 15-5
Specification Type
Standard
Specification
ASME SA747/SA747M
Specification Year
2011
Specification Status
Active
Specification Status Notes
Similar US Grade
Similar UNS Number
J92115
Equivalent Standards
Source
BPVC Section II-Materials-Part A-Ferrous Materials Specifications
Online Source
Organization
ASME International (ASME)
Available forms
Casting
Similar Alloys
Click here to find similar alloys
Links
Organizations
ASME International (ASME)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard