Layout: Alloy Finder
View
Full datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
US Customary
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
Metric
SI (Consistent)
UK Imperial
Nickel-chromium-molybdenum alloy steel, KROMITE WEAR PLATE (Associated Steel Corp.)
add data link
Chemical Composition
Base Element
Fe (Iron)
C (Carbon)
0.19
%
Cr (Chromium)
0.50
%
Fe (Iron)
96.2
%
(estimate)
Mn (Manganese)
1.20
%
Mo (Molybdenum)
0.50
%
Ni (Nickel)
1.20
%
Si (Silicon)
0.25
%
Balance
Fe (Iron)
Composition Note
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Mechanical Properties
Yield Strength
180
ksi
Ultimate Tensile Strength
199
ksi
Elongation
15
% strain
Brinell Hardness
388 to 429
Other Information
Material Class
Ferrous Alloy
Country
USA
Description
As delivered: 198,000 psi TS; 180,000 psi YS; 15 EL 45 RA; 388-429 HB; For chute liners, stamping dies, mixing blades, scraper blades.
Designation
KROMITE WEAR PLATE
Specification Type
Manufacturer's Specification
Specification Status
Active
Source
Woldman's Engineering Alloys 9th ed. J. Frick Editor, ASM International 2000
Available forms
Wrought
Similar Alloys
Click here to find similar alloys
Links
Organizations
Associated Steel Corp.
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard