Layout: Alloy Finder
View
Summary datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
US Customary
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
Metric
SI (Consistent)
UK Imperial
Boron steel, 35MnB5E, ISO 4954
add data link
Chemical Composition
Base Element
Fe (Iron)
Al (Aluminum)
0.02
% (minimum)
B (Boron)
0.0008 to 0.005
%
C (Carbon)
0.32 to 0.39
%
Fe (Iron)
97.7 to 98.6
%
(estimate)
Mn (Manganese)
1.1 to 1.4
%
P (Phosphorus)
0.035
% (maximum)
S (Sulfur)
0.035
% (maximum)
Si (Silicon)
0.4
% (maximum)
Composition Note
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Mechanical Properties
Ultimate Tensile Strength
88.5
ksi (maximum)
Other Information
Material Class
Ferrous Alloy
Alloy Family
Carbon Steel
Alloy Group
Medium-carbon steel
Alloy Sub-Group
Boron steel
Country
International
Standards Body
ISO (International)
Description
Cold-heading/cold-extruding steel wire rods, wire or bars; spheroidized ann, mech props vary with treatment
Alternate Name
formerly E7
Designation
35MnB5E
Specification Type
Standard
Specification
ISO 4954
Specification Year
1993
Specification Status
Active
Specification Status Notes
active 1993
Source
Worldwide Guide to Equivalent Irons and Steels, 5th ed. ASM International 2006
Available forms
Wrought
Similar Alloys
Click here to find similar alloys
Links
Organizations
International Organization for Standardization (ISO)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard