Chemical Composition
0.8
%  (maximum)  
13.5 to 16
%    
49.3 to 59.6
%    (estimate)
2
%  (maximum)  
1 to 1.5
%    
24 to 27
%    
0.025
%  (maximum)  
1
%  (maximum)  
1.9 to 2.35
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
102
ksi    
25
% strain    
 
Other Information
At 68 F: 146 ksi TS; 102 ksi YS; 25 El. Austenitic precipitation hardening. Vacuum arc remelted. Designed for service applications at temperatures up to 1300 F.