Layout: Alloy Finder
View
Full datasheet
Printable datasheet
Hide empty items
Record properties
Expand headings
Collapse headings
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
US Customary
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
Metric
SI (Consistent)
UK Imperial
(2xxx series) wrought aluminum-copper, NA226 (Bell Telephone Laboratories)
add data link
Chemical Composition
Base Element
Al (Aluminum)
Ag (Silver)
Al (Aluminum)
94.8 to 96
%
(estimate)
As (Arsenic)
Au (Gold)
B (Boron)
Be (Beryllium)
Bi (Bismuth)
C (Carbon)
Ca (Calcium)
Cd (Cadmium)
Ce (Cerium)
Co (Cobalt)
Cr (Chromium)
Cu (Copper)
4 to 5
%
Fe (Iron)
Ga (Gallium)
Hf (Hafnium)
In (Indium)
Li (Lithium)
Mg (Magnesium)
Mn (Manganese)
Mo (Molybdenum)
N (Nitrogen)
Na (Sodium)
Nb (Niobium)
Ni (Nickel)
P (Phosphorus)
Pb (Lead)
Pd (Palladium)
Pt (Platinum)
S (Sulfur)
Sb (Antimony)
Se (Selenium)
Si (Silicon)
Sn (Tin)
Sr (Strontium)
Ta (Tantalum)
Te (Tellurium)
Th (Thorium)
Ti (Titanium)
0.2
% (maximum)
Tl (Thallium)
V (Vanadium)
W (Tungsten)
Zn (Zinc)
Zr (Zirconium)
Balance
Al (Aluminum)
Others Total
Others Each
Other elements
Composition Note
Al is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Mechanical Properties
Tabular Data
Yield Strength
14 to 28
ksi
Ultimate Tensile Strength
32.1 to 42.1
ksi
Elongation
5 to 12
% strain
Density
Brinell Hardness
65 to 100
Vickers Hardness
Rockwell Hardness C scale
Rockwell Hardness B scale
Rockwell Hardness A scale
Rockwell 30-T scale
Rockwell 15-T scale
Condition
Notes on Mechanical Properties
Other Information
Material Class
Nonferrous Alloy
Alloy Family
Alloy Group
Alloy Sub-Group
Country
USA
Standards Body
Description
32,000-42,000 TS; 14,000-28,000 YS; 5-12 El; 65-100 HB; For light alloy parts; hardenable.
Alternate Name
Designation
NA226
Specification Type
Manufacturer's Specification
Specification
Specification Year
Specification Status
Active
Specification Status Notes
Similar US Grade
Similar UNS Number
Equivalent Standards
Source
Woldman's Engineering Alloys 9th ed. J. Frick Editor, ASM International 2000
Online Source
Organization
Available forms
Wrought
Similar Alloys
Click here to find similar alloys
Links
Organizations
Bell Telephone Laboratories
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard