Chemical Composition
0.45
%    
0.85
%    
95.7
%    (estimate)
0.75
%    
0.3
%    
2
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
149000 to 180000
psi    
180000 to 210000
psi    
330 to 400
   
 
Other Information
Heat treated: 180,000-210,000 TS; 150,000-180,000 YP; 20-25 RA; 330-400 HB; For general and structural castings, shafts, gears, housings. AISI 4340. Shock resistant.