Chemical Composition
0.9 to 1.35
%    
0.05
%  (maximum)  
12.3 to 13.3
%    
0.2
%  (maximum)  
2 to 2.5
%    
7.5 to 8.5
%    
0.01
%  (maximum)  
0.008
%  (maximum)  
0.1
%  (maximum)  
 
Mechanical Properties
DimensionsYield Strength (psi)Ultimate Tensile Strength (psi)Elongation (% strain)Brinell Hardness
Thickness, 12 in. max≥ 205000≥ 220000≥ 10≥ 430

205000
psi  (minimum)  
220000
psi  (minimum)  
10
% strain  (minimum)  
430
 (minimum)  
 