Chemical Composition
0.50
%  (maximum)  
0.05
%  (maximum)  
28.0 to 31.5
%    
0.50
%  (maximum)  
7.5 to 12.0
%    
5.0
%  (maximum)  
0.5
%  (maximum)  
1.0
%  (maximum)  
46.7 to 64.5
%    (estimate)
0.030
%  (maximum)  
0.015
%  (maximum)  
0.75
%  (maximum)  
1.0
%  (maximum)  
0.50
%  (maximum)  
0.50
%  (maximum)  
Nb+Ta 1.0 max; others 0.50 max
Ni is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
80100
psi    
30
% strain    
 
Other Information



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®