Layout: Alloy Finder
View
Summary datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
IPS (Consistent)
CGS (Consistent)
FPS (Consistent)
Metric
SI (Consistent)
UK Imperial
US Customary
410/ 416, X12Cr13, MSZ 4360 (X12Cr13, MSZ 4360 (soft ann))
add data link
Chemical Composition
Base Element
Fe (Iron)
C (Carbon)
0.09 to 0.15
%
Cr (Chromium)
12 to 14
%
Fe (Iron)
83.2 to 87.9
%
(estimate)
Mn (Manganese)
1
% (maximum)
Ni (Nickel)
0.6
% (maximum)
P (Phosphorus)
0.045
% (maximum)
S (Sulfur)
0.03
% (maximum)
Si (Silicon)
1
% (maximum)
Composition Note
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Mechanical Properties
Yield Strength
36300
psi
Ultimate Tensile Strength
65300 to 94300
psi
Elongation
20
% strain
Brinell Hardness
200
(maximum)
Other Information
Material Class
Ferrous Alloy
Alloy Family
High-Alloy Steel (Corrosion and Heat Resistant, Stainless, and Nickel Steels)
Alloy Group
Martensitic stainless steel
Alloy Sub-Group
410/ 416
Country
Hungary
Standards Body
MSZ (Hungary)
Description
Corrosion resistant; 0-100 mm; soft ann
Designation
X12Cr13
Specification Type
Standard
Specification
MSZ 4360
Specification Year
1987
Specification Status
Active
Source
Worldwide Guide to Equivalent Irons and Steels, 5th ed. ASM International 2006
Available forms
Wrought
Similar Alloys
Click here to find similar alloys
Links
Organizations
Magyar Szabvanyugyi Testulet (MSZT) (Hungarian Standards Institution)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard