Chemical Composition
0.56 to 0.64
%    
96.5 to 97.2
%    (estimate)
0.7 to 1
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
1.5 to 1.8
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
156000
psi  (minimum)  
178000
psi  (minimum)  
9
% strain  (minimum)  
363 to 429
   
 
Other Information