Layout: Alloy Finder
View
Summary datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
IPS (Consistent)
CGS (Consistent)
FPS (Consistent)
Metric
SI (Consistent)
UK Imperial
US Customary
5140/5140H, 42Cr6V1, IS 1570/4 (42Cr6V1, IS 1570/4 (limiting ruling section_3))
add data link
Chemical Composition
Base Element
Fe (Iron)
C (Carbon)
0.38 to 0.46
%
Cr (Chromium)
1.4 to 1.7
%
Fe (Iron)
96.6 to 97.5
%
(estimate)
Mn (Manganese)
0.5 to 0.8
%
Si (Silicon)
0.1 to 0.35
%
V (Vanadium)
0.07 to 0.12
%
Composition Note
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Mechanical Properties
Yield Strength
113000
psi (minimum)
Ultimate Tensile Strength
142000 to 171000
psi
Elongation
11
% strain (minimum)
Brinell Hardness
295 to 350
Other Information
Material Class
Ferrous Alloy
Alloy Family
Alloy Steel
Alloy Group
Chromium steel
Alloy Sub-Group
5140/5140H
Country
India
Standards Body
BIS (India)
Description
Alloy steel; mech props for bars and forgings hardened and tempered (oil hardened); limiting ruling section 30 mm.
Designation
42Cr6V1
Specification Type
Standard
Specification
IS 1570/4
Specification Year
2001
Specification Status
Active
Specification Status Notes
active 2001
Source
Worldwide Guide to Equivalent Irons and Steels, 5th ed. ASM International 2006
Available forms
Wrought
Similar Alloys
Click here to find similar alloys
Links
Organizations
Bureau of Indian Standards (BIS)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard