Chemical Composition
0.02
%    
18.5
%    
63.2
%    (estimate)
1
%    
3.5
%    
13
%    
0.8
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
68000
psi    
88500
psi    
35
% strain    
 
Other Information
Shielded metal-arc welding electrode for welding types 317 and 317L and where improved corrosion resistance over E316L is required. 88,500 psi TS; 68,000 psi YS; 35% El.
EUTECTRODE E317L-16
 