Chemical Composition
0.45
%  (maximum)  
0.5
%    
97.1 to 97.5
%    (estimate)
0.95
%    
0.5
%    
0.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
95000 to 125000
psi    
120000 to 149000
psi    
9 to 14
% strain    
290 to 350
   
 
Other Information
Cast: 120,000-150,000 TS; 95,000-125,000 YP; 9-14 El; 22-30 RA; 290-350 HB; For general and structural castings, shafts, gears, housings. High strength, shock resistant. AISI 8640 modified.