Chemical Composition
0.3
%    
98.9 to 99.1
%    (estimate)
0.6 to 0.8
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
52900 to 98000
psi    
80100 to 128000
psi    
10 to 30
% strain    
165 to 250
   
 
Other Information
Links
Organizations

 



No warranty is given for the accuracy of these data