Chemical Composition
0.07
%    
17 to 19
%    
69.1 to 73.6
%    (estimate)
0.6
%    
8 to 10.5
%    
0.75
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
4.32e6
lbf/ft^2    
1.08e7
lbf/ft^2    
35
% strain    
200
   
 
Other Information
Links