Range attributes
0.9 to 1.35
%    
430
 (minimum)  
0.05
%  (maximum)  
12.3 to 13.3
%    
10
% strain  (minimum)  
0.2
%  (maximum)  
2 to 2.5
%    
7.5 to 8.5
%    
0.01
%  (maximum)  
0.008
%  (maximum)  
0.1
%  (maximum)  
3.17e7
lbf/ft^2  (minimum)  
2.95e7
lbf/ft^2  (minimum)  
 
Discrete attributes
Short text attributes
S13800 Type XM-13
ASME SA705/SA705M
 
Long text attributes
Age-hardening stainless steel forgings, Condition H950
ASME International (ASME)
 
Hyperlink attributes
Integer attributes
Tabular attributes
DimensionsYield Strength (lbf/ft^2)Ultimate Tensile Strength (lbf/ft^2)Elongation (% strain)Brinell Hardness
Thickness, 12 in. max≥ 2.95e7≥ 3.17e7≥ 10≥ 430

 
Further Information
 



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®