Layout: No layout
View
Full datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Expand all metadata
Collapse all metadata
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
FPS (Consistent)
CGS (Consistent)
IPS (Consistent)
Metric
SI (Consistent)
UK Imperial
US Customary
Grade WP S31254, ASME SA403/SA403M, Fitting; longitudinal
add data link
Range attributes
C (Carbon)
0.02
% (maximum)
Cr (Chromium)
19.5 to 20.5
%
Cu (Copper)
0.5 to 1
%
Elongation
28
% strain (minimum)
Mn (Manganese)
1
% (maximum)
Mo (Molybdenum)
6 to 6.5
%
Ni (Nickel)
17.5 to 18.5
%
P (Phosphorus)
0.03
% (maximum)
S (Sulfur)
0.01
% (maximum)
Si (Silicon)
0.8
% (maximum)
Ultimate Tensile Strength
1.35e7 to 1.71e7
lbf/ft^2
Yield Strength
6.34e6
lbf/ft^2 (minimum)
Discrete attributes
~Checking Status
Verified - New record
Date Last Checked
Monday, January 8, 2018
Alloy Family
High-Alloy Steel (Corrosion and Heat Resistant, Stainless, and Nickel Steels)
Alloy Group
Austenitic stainless steel
Alloy Sub-Group
F44
Base Element
Fe (Iron)
Country
USA
Material Class
Ferrous Alloy
Source
BPVC Section II-Materials-Part A-Ferrous Materials Specifications
Specification Status
Active
Specification Type
Standard
Standards Body
ASME (USA)
Short text attributes
Alternate Name
Grade CR S31254
Designation
Grade WP S31254
Similar UNS Number
S31254
Specification
ASME SA403/SA403M
Long text attributes
Description
Wrought austenitic stainless steel piping fittings for pressure piping applications; longitudinal
Notes on Mechanical Properties
Elongation in 4 D
Organization
ASME International (ASME)
Other elements
N2C = 0.18 to 0.22
Hyperlink attributes
Similar Alloys
Click here to find similar alloys
Integer attributes
Specification Year
2011
Tabular attributes
Tabular Data
Hide table
Save as CSV
Copy To Clipboard
Dimensions
Yield Strength (lbf/ft^2)
Ultimate Tensile Strength (lbf/ft^2)
Elongation (% strain)
None Specified
≥ 6.34e6
1.35e7 to 1.71e7
≥ 28
Save as CSV
Copy To Clipboard
Further Information
Organizations
ASME International (ASME)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard