Layout: No layout
View
Full datasheet
Printable datasheet
Hide empty items
Record properties
Expand headings
Collapse headings
Expand all metadata
Collapse all metadata
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
FPS (Consistent)
CGS (Consistent)
IPS (Consistent)
Metric
SI (Consistent)
UK Imperial
US Customary
CB7Cu-2 Type 15-5, ASME SA747/SA747M, Casting; H1150M
add data link
Range attributes
Ag (Silver)
Al (Aluminum)
As (Arsenic)
Au (Gold)
B (Boron)
Be (Beryllium)
Bi (Bismuth)
Brinell Hardness
310
(minimum)
C (Carbon)
0.07
% (maximum)
Ca (Calcium)
Cd (Cadmium)
Ce (Cerium)
Co (Cobalt)
Cr (Chromium)
14 to 15.5
%
Cu (Copper)
2.5 to 3.2
%
Density
Elongation
Fe (Iron)
Ga (Gallium)
Hf (Hafnium)
In (Indium)
Li (Lithium)
Mg (Magnesium)
Mn (Manganese)
0.7
% (maximum)
Mo (Molybdenum)
N (Nitrogen)
0.05
% (maximum)
Na (Sodium)
Nb (Niobium)
0.15 to 0.35
%
Ni (Nickel)
4.5 to 5.5
%
Others Each
Others Total
P (Phosphorus)
0.035
% (maximum)
Pb (Lead)
Pd (Palladium)
Pt (Platinum)
Rockwell 15-T scale
Rockwell 30-T scale
Rockwell Hardness A scale
Rockwell Hardness B scale
Rockwell Hardness C scale
S (Sulfur)
0.03
% (maximum)
Sb (Antimony)
Se (Selenium)
Si (Silicon)
1
% (maximum)
Sn (Tin)
Sr (Strontium)
Ta (Tantalum)
Te (Tellurium)
Th (Thorium)
Ti (Titanium)
Tl (Thallium)
Ultimate Tensile Strength
V (Vanadium)
Vickers Hardness
W (Tungsten)
Yield Strength
Zn (Zinc)
Zr (Zirconium)
Logical attributes
Bar
Bearing
Billet
Bloom
Casting
Export?
Extrusion
Foil
Forging
Ingot
None Specified
Other
Pipe
Plate
Rod
Shaft
Sheet
Spring
Strip
Tube
Wire
Discrete attributes
~Checking Status
Verified - New record
Date Last Checked
Monday, January 8, 2018
Checked By
Notes
Alloy Family
High-Alloy Steel (Corrosion and Heat Resistant, Stainless, and Nickel Steels)
Alloy Group
Precipitation-hardening stainless steel
Alloy Sub-Group
Miscellaneous precipitation-hardening steels
Available forms
Casting
Balance
Base Element
Fe (Iron)
Country
USA
Material Class
Ferrous Alloy
Source
BPVC Section II-Materials-Part A-Ferrous Materials Specifications
Specification Status
Active
Specification Type
Standard
Standards Body
ASME (USA)
Short text attributes
Alternate Name
Composition Note_old
Country*
Deoxidation Method
Description_old
Designation
CB7Cu-2 Type 15-5
Equivalent Standards_old
Filing Code
Material Number
Other elements_old
Similar UNS Number
J92116
Similar US Grade
Specification
ASME SA747/SA747M
Specification Status Notes
Long text attributes
Composition Note
Condition
Description
Steel castings, stainless, precipitation hardening; PH Heat Treatment H1150M
Equivalent Standards
Notes on Mechanical Properties
Organization
ASME International (ASME)
Other elements
Hyperlink attributes
Online Source
Similar Alloys
Click here to find similar alloys
Integer attributes
ID
Source ID
Specification Year
2011
Tabular attributes
Tabular Data
Hide table
Save as CSV
Copy To Clipboard
Dimensions
Yield Strength (lbf/ft^2)
Ultimate Tensile Strength (lbf/ft^2)
Elongation (% strain)
Brinell Hardness
Rockwell 30-T scale
Treatment
Hardness Scale
Vickers hardness (HV)
None Specified
≥ 310
Save as CSV
Copy To Clipboard
Further Information
Organizations
ASME International (ASME)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard