Chemical Composition
0.17 to 0.23
%    
0.35 to 0.7
%    
0.4
%  (maximum)  
96.3 to 98.1
%    (estimate)
0.65 to 0.95
%    
0.15 to 0.25
%    
0.4 to 0.7
%    
0.025
%  (maximum)  
0.035
%  (maximum)  
0.15 to 0.4
%    
1) Cast analysis.
2) The steel shall be supplied in the killed condition.
3) For steels with hardenability requirements, except for P and S, insignificant deviations from the limits for cast analysis are permissible; these deviations shall, however, not exceed in the case of carbon ±0.01 % and in all other cases the values according to ISO 683-3 – Table 4.
4) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulfide morphology) or Pb additions may be supplied on request. In the first case, the upper limit for the Mn content may be increased by 0.15 %.
5) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
1) Cast analysis.
2) The steel shall be supplied in the killed condition.
3) For steels with hardenability requirements, except for P and S, insignificant deviations from the limits for cast analysis are permissible; these deviations shall, however, not exceed in the case of carbon ±0.01 % and in all other cases the values according to ISO 683-3 – Table 4.
4) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulfide morphology) or Pb additions may be supplied on request. In the first case, the upper limit for the Mn content may be increased by 0.15 %.
5) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
DimensionsBrinell Hardness
None Specified149 to 194

149 to 194
   
Treated to ferrite-pearlite structure (+FP)
 
Other Information
Links



No warranty is given for the accuracy of these data