Chemical Composition
0.18 to 0.25
%    
0.4
%  (maximum)  
0.3
%  (maximum)  
96.5 to 98.4
%    (estimate)
1.3 to 1.65
%    
0.4
%  (maximum)  
0.025
%  (maximum)  
0.035
%  (maximum)  
0.1 to 0.4
%    
1) Cast analysis.
2) The steel shall be supplied in the killed condition.
3) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulfide morphology) or Pb additions may be supplied on request. In the first case, the upper limit for the Mn content may be increased by 0.15 %.
4) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
DimensionsBrinell Hardness
None Specified149 to 197

149 to 197
   
Treated to hardness range (+TH)
 
Other Information
Links