Layout: No layout
View
Summary datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Expand all metadata
Collapse all metadata
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
FPS (Consistent)
CGS (Consistent)
IPS (Consistent)
Metric
SI (Consistent)
UK Imperial
US Customary
46S20, ISO 683-18, Bar, +C temper
add data link
Range attributes
C (Carbon)
0.42 to 0.5
%
Elongation
8
% strain (minimum)
Fe (Iron)
97.7 to 98.7
%
(estimate)
Mn (Manganese)
0.7 to 1.1
%
P (Phosphorus)
0.06
% (maximum)
S (Sulfur)
0.15 to 0.25
%
Si (Silicon)
0.4
% (maximum)
Ultimate Tensile Strength
1.21e7 to 1.71e7
lbf/ft^2
Yield Strength
7.1e6
lbf/ft^2 (minimum)
Discrete attributes
~Checking Status
Verified - New record
Date Last Checked
Monday, January 8, 2018
Alloy Family
Carbon Steel
Alloy Group
Medium-carbon steel
Alloy Sub-Group
1145/ 1146
Available forms
Bar
Balance
Fe (Iron)
Base Element
Fe (Iron)
Country
International
Material Class
Ferrous Alloy
Specification Status
Active
Specification Type
Standard
Standards Body
ISO (International)
Short text attributes
Designation
46S20
Specification
ISO 683-18
Long text attributes
Composition Note
1) Cast analysis.
2) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Condition
Cold drawn (+C temper)
Description
Bright steel products
Organization
International Organization for Standardization (ISO)
Hyperlink attributes
Similar Alloys
Click here to find similar alloys
Integer attributes
Specification Year
2014
Tabular attributes
Tabular Data
Hide table
Save as CSV
Copy To Clipboard
Dimensions
Yield Strength (lbf/ft^2)
Ultimate Tensile Strength (lbf/ft^2)
Elongation (% strain)
Thickness, ≥ 5 to ≤ 10 mm
≥ 1.19e7
1.55e7 to 2.05e7
≥ 5
Thickness, > 10 to ≤ 16 mm
≥ 9.82e6
1.44e7 to 1.94e7
≥ 6
Thickness, > 16 to ≤ 40 mm
≥ 8.35e6
1.34e7 to 1.84e7
≥ 7
Thickness, > 40 to ≤ 63 mm
≥ 7.94e6
1.27e7 to 1.78e7
≥ 8
Thickness, > 63 to ≤ 100 mm
≥ 7.1e6
1.21e7 to 1.71e7
≥ 8
Save as CSV
Copy To Clipboard
Further Information
Organizations
International Organization for Standardization (ISO)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard