Chemical Composition
0.42 to 0.5
%    
0.4
%  (maximum)  
0.3
%  (maximum)  
97 to 99
%    (estimate)
0.5 to 0.8
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.025
%  (maximum)  
0.035
%  (maximum)  
0.1 to 0.4
%    
Cr + Mo + Ni ≤ 0.63 %
1) Cast analysis.
2) The steel shall be supplied in the killed condition.
3) Steel may be supplied with a lower Si content. In this case, alternative means of deoxidation shall be used.
4) In the case of grades with specified hardenability requirements, except for P and S, insignificant deviations from the limits for cast analysis are permissible; these deviations shall, however, not exceed in the case of C ±0.01 %, and in all other cases, the values according to ISO 683-1 – Table 4.
5) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulphide morphology) or Pb additions may be available on request. In the first case, the upper limit for the Mn content may be increased by 0.15 %.
6) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
DimensionsYield Strength (lbf/ft^2)Ultimate Tensile Strength (lbf/ft^2)Elongation (% strain)
Diameter or thickness, ≤ 16 mm≥ 7.1e6≥ 1.29e7≥ 14
Diameter or thickness, > 16 to ≤ 100 mm≥ 6.37e6≥ 1.21e7≥ 16
Diameter or thickness, > 100 to ≤ 250 mm≥ 5.74e6≥ 1.17e7≥ 16

5.74e6
lbf/ft^2  (minimum)  
1.17e7
lbf/ft^2  (minimum)  
16
% strain  (minimum)  
Normalized (+N temper)
Mechanical properties for products with a diameter or thickness > 100 mm to ≤ 250 mm.
 