Chemical Composition
0.22 to 0.29
%    
0.4
%  (maximum)  
0.3
%  (maximum)  
97.3 to 99.3
%    (estimate)
0.4 to 0.7
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.045
%  (maximum)  
0.045
%  (maximum)  
0.1 to 0.4
%    
Cr + Mo + Ni ≤ 0.63 %
1) Cast analysis.
2) The steel shall be supplied in the fully killed condition.
3) Steels may be supplied with a lower silicon content. In this case, alternative means of deoxidation shall be used.
4) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulfide morphology) or Pb additions may be supplied on request. In the first case, the upper limit for the Mn content may be increased by 0.15 %.
5) Cu content above 0.40 % can cause hot shortness during hot forming.
6) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
DimensionsUltimate Tensile Strength (lbf/ft^2)Brinell Hardness
Thickness, > 16 to ≤ 40 mm9.19e6 to 1.34e7131 to 187
Thickness, > 40 to ≤ 63 mm9.19e6 to 1.34e7131 to 187
Thickness, > 63 to ≤ 100 mm9.19e6 to 1.34e7131 to 187

9.19e6 to 1.34e7
lbf/ft^2    
131 to 187
   
As-rolled, peeled (+SH)
 