Chemical Composition
0.12 to 0.18
%    
0.4
%  (maximum)  
0.3
%  (maximum)  
97.6 to 99.4
%    (estimate)
0.3 to 0.6
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.025
%  (maximum)  
0.02 to 0.04
%    
0.15 to 0.4
%    
1) Cast analysis.
2) The steel shall be supplied in the killed condition.
3) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulfide morphology) or Pb additions may be supplied on request. In the first case, the upper limit for the Mn content may be increased by 0.15 %.
4) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
DimensionsBrinell Hardness
None Specified≤ 143

143
 (maximum)  
Soft annealed (+A temper)
 
Other Information
Links