Chemical Composition
0.12 to 0.18
%    
0.4
%  (maximum)  
0.3
%  (maximum)  
97.6 to 99.4
%    (estimate)
0.3 to 0.6
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.025
%  (maximum)  
0.02 to 0.04
%    
0.15 to 0.4
%    
1) Cast analysis.
2) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulphide morphology) or Pb additions may be available on request. In the first case, the upper limit of the Mn-content may be increased by 0.15 %.
3) Steels may be supplied with a lower Si content. In this case, alternative means of deoxidation shall be used.
4) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
DimensionsYield Strength (lbf/ft^2)Ultimate Tensile Strength (lbf/ft^2)Elongation (% strain)
Thickness, ≥ 5 to ≤ 10 mm≥ 7.94e61.04e7 to 1.67e7≥ 7
Thickness, > 10 to ≤ 16 mm≥ 7.1e61e7 to 1.63e7≥ 8
Thickness, > 16 to ≤ 40 mm≥ 5.85e68.98e6 to 1.52e7≥ 9
Thickness, > 40 to ≤ 63 mm≥ 5.01e67.94e6 to 1.4e7≥ 11
Thickness, > 63 to ≤ 100 mm≥ 4.49e67.1e6 to 1.25e7≥ 12

4.49e6
lbf/ft^2  (minimum)  
7.1e6 to 1.25e7
lbf/ft^2    
12
% strain  (minimum)  
Cold drawn (+C temper)
 
Other Information