Chemical Composition
0.14
%  (maximum)  
97.8 to 98.7
%    (estimate)
1 to 1.5
%    
0.11
%  (maximum)  
0.34 to 0.4
%    
0.05
%  (maximum)  
1) Cast analysis.
2) Since, Si has an adverse effect on machinability, it is not intentionally added to specified limits, but if the formation of special oxides is guaranteed, a Si content of 0.10-0.40 % may be agreed.
3) At the time of enquiry and order, it may be agreed that either a grade with 0.06-0.11 % P or a grade with  0.05 % P shall be delivered.
4) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
DimensionsUltimate Tensile Strength (lbf/ft^2)Brinell Hardness
Thickness, > 16 to ≤ 40 mm7.94e6 to 1.19e7≤ 169
Thickness, > 40 to ≤ 63 mm7.73e6 to 1.19e7≤ 169
Thickness, > 63 to ≤ 100 mm7.52e6 to 1.09e7≤ 154

7.52e6 to 1.09e7
lbf/ft^2    
154
 (maximum)  
As-rolled, peeled (+SH)
 
Other Information
Links



No warranty is given for the accuracy of these data