Chemical Composition
0.47 to 0.55
%    
0.4
%  (maximum)  
0.3
%  (maximum)  
96.9 to 98.8
%    (estimate)
0.6 to 0.9
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.045
%  (maximum)  
0.045
%  (maximum)  
0.1 to 0.4
%    
Cr + Mo + Ni ≤ 0.63 %
1) Cast analysis.
2) The steel shall be supplied in the killed condition.
3) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulphide morphology) or Pb additions may be available on request. In the first case, the upper limit for the Mn content may be increased by 0.15 %.
4) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
DimensionsBrinell Hardness
None Specified≤ 255

255
 (maximum)  
Treated to improve shearability (+S temper)
 