Chemical Composition
0.37 to 0.44
%    
0.4
%  (maximum)  
0.3
%  (maximum)  
97.1 to 99
%    (estimate)
0.5 to 0.8
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.045
%  (maximum)  
0.045
%  (maximum)  
0.1 to 0.4
%    
Cr + Mo + Ni ≤ 0.63 %
1) Cast analysis.
2) The steel shall be supplied in the killed condition.
3) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulphide morphology) or Pb additions may be available on request. In the first case, the upper limit for the Mn content may be increased by 0.15 %.
4) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
DimensionsYield Strength (lbf/ft^2)Ultimate Tensile Strength (lbf/ft^2)Elongation (% strain)
Diameter or thickness, ≤ 16 or ≤ 8 mm respectively≥ 9.61e61.36e7 to 1.67e7≥ 16
Diameter or thickness, > 16 to ≤ 40 or > 8 to ≤ 20 mm respectively≥ 8.35e61.32e7 to 1.63e7≥ 18
Diameter or thickness, > 40 to ≤ 100 or > 20 to ≤ 60 mm respectively≥ 7.31e61.25e7 to 1.57e7≥ 19

7.31e6
lbf/ft^2  (minimum)  
1.25e7 to 1.57e7
lbf/ft^2    
19
% strain  (minimum)  
Quenched and tempered (+QT)
Mechanical properties for ruling sections with a diameter > 40 mm to ≤ 100 mm, or for flat products with a thickness > 20 mm to ≤ 60 mm.
 
Other Information