Chemical Composition
0.32 to 0.39
%    
0.4
%  (maximum)  
0.3
%  (maximum)  
97.1 to 99.1
%    (estimate)
0.5 to 0.8
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.025
%  (maximum)  
0.02 to 0.04
%    
0.1 to 0.4
%    
Cr + Mo + Ni ≤ 0.63 %
1) Cast analysis.
2) The steel shall be supplied in the killed condition.
3) Steel may be supplied with a lower Si content. In this case, alternative means of deoxidation shall be used.
4) In the case of grades with specified hardenability requirements, except for P and S, insignificant deviations from the limits for cast analysis are permissible; these deviations shall, however, not exceed in the case of C ±0.01 %, and in all other cases, the values according to ISO 683-1 – Table 4.
5) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulphide morphology) or Pb additions may be available on request. In the first case, the upper limit for the Mn content may be increased by 0.15 %.
6) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
48
 (minimum)  
Quenched and tempered, surface hardened, stress relieved or normalized, surface hardened, stress relieved (+QT+SR or N+SR)