Chemical Composition
0.32 to 0.39
%    
0.4
%  (maximum)  
0.3
%  (maximum)  
97.2 to 99.1
%    (estimate)
0.5 to 0.8
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.025
%  (maximum)  
0.035
%  (maximum)  
0.1 to 0.4
%    
Cr + Mo + Ni ≤ 0.63 %
1) Cast analysis.
2) The steel shall be supplied in the killed condition.
3) Steel may be supplied with a lower Si content. In this case, alternative means of deoxidation shall be used.
4) In the case of grades with specified hardenability requirements, except for P and S, insignificant deviations from the limits for cast analysis are permissible; these deviations shall, however, not exceed in the case of C ±0.01 %, and in all other cases, the values according to ISO 683-1 – Table 4.
5) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulphide morphology) or Pb additions may be available on request. In the first case, the upper limit for the Mn content may be increased by 0.15 %.
6) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
DimensionsYield Strength (lbf/ft^2)Ultimate Tensile Strength (lbf/ft^2)Elongation (% strain)
Diameter or thickness, ≤ 16 or ≤ 8 mm respectively≥ 8.98e61.32e7 to 1.63e7≥ 17
Diameter or thickness, > 16 to ≤ 40 or > 8 to ≤ 20 mm respectively≥ 7.94e61.25e7 to 1.57e7≥ 19
Diameter or thickness, > 40 to ≤ 100 or > 20 to ≤ 60 mm respectively≥ 6.68e61.15e7 to 1.46e7≥ 20

6.68e6
lbf/ft^2  (minimum)  
1.15e7 to 1.46e7
lbf/ft^2    
20
% strain  (minimum)  
Quenched and tempered (+QT)
Mechanical properties for ruling sections with a diameter > 40 mm to ≤ 100 mm, or for flat products with a thickness > 20 mm to ≤ 60 mm.
 