Chemical Composition
0.27 to 0.34
%    
0.4
%  (maximum)  
0.3
%  (maximum)  
97.2 to 99.1
%    (estimate)
0.5 to 0.8
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.045
%  (maximum)  
0.045
%  (maximum)  
0.1 to 0.4
%    
Cr + Mo + Ni ≤ 0.63 %
1) Cast analysis.
2) The steel shall be supplied in the fully killed condition.
3) Steels may be supplied with a lower silicon content. In this case, alternative means of deoxidation shall be used.
4) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulfide morphology) or Pb additions may be supplied on request. In the first case, the upper limit for the Mn content may be increased by 0.15 %.
5) Cu content above 0.40 % can cause hot shortness during hot forming.
6) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
DimensionsYield Strength (lbf/ft^2)Ultimate Tensile Strength (lbf/ft^2)Elongation (% strain)
Thickness, ≥ 5 to ≤ 10 mm≥ 9.5e61.27e7 to 1.9e7≥ 6
Thickness, > 10 to ≤ 16 mm≥ 8.77e61.19e7 to 1.82e7≥ 7
Thickness, > 16 to ≤ 40 mm≥ 7.21e61.15e7 to 1.78e7≥ 8
Thickness, > 40 to ≤ 63 mm≥ 6.27e61.09e7 to 1.71e7≥ 9
Thickness, > 63 to ≤ 100 mm≥ 5.22e61e7 to 1.63e7≥ 9

5.22e6
lbf/ft^2  (minimum)  
1e7 to 1.63e7
lbf/ft^2    
9
% strain  (minimum)  
Cold drawn (+C temper)
 
Other Information
Links



No warranty is given for the accuracy of these data