Chemical Composition
0.04
%  (maximum)  
19 to 22
%    
1 to 3
%    
39.5 to 52
%    (estimate)
2.5
%  (maximum)  
4 to 6
%    
24 to 26
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
0.9
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1.17e7
lbf/ft^2  (minimum)  
22
% strain  (minimum)  
 
Other Information