Chemical Composition
0.32
%  (maximum)  
97.7 to 98
%    (estimate)
1.5
%    
0.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
7.21e6 to 1.3e7
lbf/ft^2    
1.15e7 to 1.73e7
lbf/ft^2    
14 to 22
% strain    
150 to 210
   
 
Other Information
Cast: 80,000-120,000 TS; 50,000-90,000 YS; 14-22 El; 150-210 HB; 30-35 RA. For general and structural applications, gears, housings. Good weldability. ASTM A148.