Chemical Composition
0.3
%  (maximum)  
99 to 99.3
%    (estimate)
0.7
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
5.03e6 to 7.92e6
lbf/ft^2    
9.36e6 to 1.15e7
lbf/ft^2    
24 to 30
% strain    
125 to 160
   
 
Other Information
Cast: 65,000-80,000 TS; 35,000-55,000 YP; 125-160 HB; 24-30 El. For general and structural applications, gears, housings. Excellent weldability. AISI 1025.